PA66美国杜邦408HS纯树脂
体积电阻率 | DAM|50%RH10|10 | Ω.cm | ASTM D-257 |
介电常数 (10Hz(cps)) | DAM|50%RH3.1|4.8 | ASTM D-150 | |
耗散因数 | ASTM D-150 | ||
(100Hz(cps)) | DAM|50%RH0.02|0.1 | ||
(10Hz(cps)) | DAM|50%RH0.02|0.11 | ||
(10Hz(cps)) | DAM|50%RH0.02|0.10 | ||
介电常数 | ASTM D-150 | ||
(100Hz(cps)) | DAM|50%RH3.1|5.9 | ||
(10Hz(cps)) | DAM|50%RH2.9|3.3 |
热畸变温度 ((0.5)×10Pa) | DAM|50%RH230|- | ℃ | ASTM D-648 |
UL可燃性导级 | DAM|50%RH94|HB | UL 94 | |
熔点结晶 | DAM|50%RH270|- | ℃ | ASTM D-2177 |
线性热膨胀系数 | DAM|50%RH7×10-5|- | m/m/℃ | ASTM D-696 |
荷重形变 (13.8MPa.50℃) | DAM|50%RH1.4|- | % | ASTM D-621 |
熔点 (Fisher Johns法) | DAM|50%RH255|255 | ℃ | ASTM D-789 |
热畸变温度 (18×10Pa) | DAM|50%RH75|- | ℃ | ASTM D-648 |
脆化温度 | DAM|50%RH-104|-84 | ℃ | ASTM D-746 |
需氧指数 | DAM|50%RH19|20 | % | ASTM D-2863 |